Re the sunburn peel paint...its going to be either Johnstons or Leyland , both of which I've used in the past with no issues. It's odd because the worst peel areas are in sunlight near windows or doors, uv light breaking it down perhaps or it just might be poor prep that time...or dodgy paint, who knows?
Deluxe water based this time, cheap Wickes sander did speed things up an awful lot, lots to do but a busy period coming up with a mask fitting session for my wife's radiotherapy then 10 sessions following.
She asked, why are you starting it now

? You know we're going to be busy ?
Because it's been doing my head in...I do get aggravated putting things off, which I have been but am not motivated to start. Eventually I get so aggravated it's easier to start than put it off any longer. Anyone else.like this ?